INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

valve casting radiography

valve casting radiography

valve casting radiography

(OP)
Does anyone have a good document on QA/QC for valve casting radiography?  I'm trying to write one for my company and it is difficult decyphering the various standards.  THANKS

RE: valve casting radiography

I'd suggest ASME B16.34 as a good place to start.  Annex Bn lists radiographic acceptance standards, and refers to some ASTM documents that may be helpful (E94, E142).  Figures 6-14 show typicla valve casting sections requiring radiography.

I hope this helps.

Jonathan Nieuwsma

RE: valve casting radiography

I suggest the following document from the Manufacturers Standardization Society.  SP-54 Quality Standard for Steel Castings for Valves, Flanges, and Fittings and Other Piping Components - Radiographic Examination Method

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources