INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Aplication procedures

Aplication procedures

Aplication procedures

(OP)
HIya,
I was wondering if anyone could shed any light on different application procedures of galvanising? Is it possible to buy it in an aerosal form? I recently saw a site advertising it in aerosal form, cant remember where though.
Also recently heard someone talking about cold dip galvanising. Does anyone know about this?
Many thanks

RE: Aplication procedures

Galavanizing is done predominantly by electroplating zinc on steel or by dipping steel in molten zinc. Applying it by other means would work, in theory, if the zinc is in electrical contact with the steel and has adequate coverage. I honestly don't know if any such method exists.

RE: Aplication procedures

If you do a google search on cold galvanizing, you will find several possibilities.  There is also a mechanical galvanizing process that may be of interest.  Again, google it.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources