INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

aluminum alloys

aluminum alloys

aluminum alloys

(OP)
can 6061 and 6063 aluminum alloys welded to each other?

Thanks

V2

RE: aluminum alloys

Yes, they can. Table 1.2 in ANSI/AWS D1.2-97 indicates that a 4043 electrode can be used with footnotes for several other acceptable rods.  Table 7.2-1 in "Specifications for Aluminum Structures - ASD", Seventh Ed. indicates a 5356 electode. Again it has a footnotes with other electrodes that can be used. 4043 is among them.

I'm not expert enough to suggest a particular rod.  Besides who ever is would need a lot more information.

HTH

RE: aluminum alloys

We use 4043 wire unless the service temperature is over 150 DegF

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources