Annealing Aluminium
Annealing Aluminium
(OP)
Can anyone tell me where I can get curves showing the effect on Room Temperature UTS & Proof strength of 2014-T651 Aluminium alloy, after being subjected to a particular temperature-time history? I am coating some parts with Rilsan nylon at 310C for 15 minutes. ESDU data sheets only go up to 250C. MIL-HDBK-5 only has room temp. data for 2024-T3.





RE: Annealing Aluminium
Properties of Aluminum Alloys: Tensile, Creep and Fatigue Data at High and Low Temperatures
http://www.asminternational.org/Template.cfm?Section=BrowsebyTopic&template=Ecommerce/ProductDisplay.cfm&ProductID=11205
If it isn't in this book, then try Alcoa or Alcan. They may have unpublished data on this.