INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Japanese Steel Plate Quality

Japanese Steel Plate Quality

Japanese Steel Plate Quality

(OP)
Could anyone help me find the specification sheets of a Japanese steel grade called SM41B?

Is there any website where one could just go and look up Unassigned ASME material?

I would appreciate the assistance.

Kind regards,

RE: Japanese Steel Plate Quality

SM41B is the former name of SM400B  per G 3106.
This is a weldable structural steel . Carbon content is below 0.20%.

RE: Japanese Steel Plate Quality

SM41B crosslists to the European standards EN10025/S235J0(1.0114).  It appears to be a low carbon structural steel similar to ASTM A36 except with a minimum toughness requirement of 25 J (Charpy test). http://www.steelstructures.com/IIW%20files/JIS%20ASTM%20EN%20materials%20comparison%20-%20Horikawa.xls

JIS        ASTM      EN                   
SM41B    A36(*)    EN10025/S235J0(1.0114)
    (*)minmum Charpy requirement 25J

The cross-listing of steels at the following site doesn’t list SM41B; perhap it’s been replaced by G3106?
http://www.isteelasia.com/tools/tool552.jsp

JIS G3106  Rolled steel for welded structure  
EN 10025-90 Hot-rolled products of non-alloy structural steels-Technical delivery conditions

There’s a mention of some SM41B fatigue properties (from Trinity College in Ireland) at
http://www.mme.tcd.ie/Groups/Materials/SampleReport.htm

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources