INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Precipitate the heavy metal from EDTA complex

Precipitate the heavy metal from EDTA complex

Precipitate the heavy metal from EDTA complex

(OP)
We want to precipitate the nickel ion from complex EDTA-nickel by hydroxide (OH from lime) but did not  work ! The EDTA-Ni is so stable,  Ni ion can not form a complex with OH to be precipitate ! !.

 We try to break down the EDTA-Ni complex before precipitate by oxidation (HNO3/H2O2, Hypochlorite, O3/UV, thermal hydrolysis ..., ) but Ni can not be free from EDTA !   

Any body who know how to precipitate the heavy metal from EDTA complex (EDTA-m) please let we know !!.

Thanks

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources