INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Free sources for material property data
5

Free sources for material property data

Free sources for material property data

(OP)
What are some good free sources for material property data? In particular I'm looking for info on a broad range of stainless steels.

The ASM volumes are an option but they aren't at ready use. Are there any sites you'd recommend. I want to find some information for a broad range of grades.

RE: Free sources for material property data

SSINA (Specialty Steel Industry of North America) is an excellent source of information on stainless steels.  Check out their publications section:

http://www.ssina.com

As NickE mentioned, Carpenter (http://www.cartech.com) is an excellent source of information.  Other manufacturers of stainless steel with technical information on their websites include the following:

Allegheny Ludlum
http://www.alleghenyludlum.com

AK Steel
http://www.aksteel.com

AvestaPolarit
http://www.avestapolarit.com/

Sandvik
http://www.steel.sandvik.com/

ThyssenKrupp Nirosta
http://www.nirosta.de/nirosta/index.html?lang=en

RE: Free sources for material property data

Another excellent source of SS info is the Nickel Development Institute,
http://www.nidi.org/index.cfm/ci_id/9/la_id/1.htm
with 375 technical papers, etc., as free downloads.

Another great source (& easy to navigate) is the Stainless Steel Property Database at
http://www.hghouston.com/ssdata.html

Stainless Plate Products has less content, but you can find info, shapes & stock quickly for standard grades of SS:
http://www.sppusa.com/reference/stainless_steel/steel.html

Here's a concise page on SS welding electrodes:
http://www.kakani.com/w-stainless_steel_welding_electrod.html

Here's a description of Basic Mill Plate Finishes for Stainless Steel, with surface roughness values Ra
http://www.delstar.com/services/quality/mill.html

Atlas Steel has a straightforward site for SS tech. info:
http://www.atlas-steels.com.au/techinfo/index.html

Edstrom is a specialized site dealing with SS water sytems; deals with chlorination, bacteria, corrosion, lab water:
http://www.edstrom.com/Resources.cfm?doc_id=129

Finally, honorable mention goes to the Australian Stainless Steel Development Association
http://www.assda.asn.au/

RE: Free sources for material property data

This thread should be made into a Comprehensive listing... We could all use a list of the man and varied free list of materials data sources.. i've found out about several through this board...

Hmmmm ..

When I get some free time I'll try and compile a list.....

I'll post here for edits and addendums.

Nick

RE: Free sources for material property data

(OP)
Thanks for the links guys.

Yeah I'm actually making my own little web page full of good links. I just want the best of course. Sometimes you notice people with a web page full of way too many links. It's hard to know what is useful.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources