INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

S-N Curves for Bolted Joints - need good reference

S-N Curves for Bolted Joints - need good reference

S-N Curves for Bolted Joints - need good reference

(OP)
I am looking for a reference with S-N curves for bolted joints.  The joint we're considering would be like a diving board with a bolted support, so the bolts could see a prying action.  Does anyone know of a good reference for those curves?

RE: S-N Curves for Bolted Joints - need good reference

I would contact the bolt manufacturer.
A good rule of thumb is .57 x the
maximum tensile strength for dynamic
applications.  The manufacturer should
have run many tests on their bolts and
have this information available.

RE: S-N Curves for Bolted Joints - need good reference

BS7608 has what you require

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources