INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Flow drilling??

Flow drilling??

Flow drilling??

(OP)
I hope I'm in the correct forum,
Can anyone tell me where I might find information about the flow dilling process.
Information about suppliers for components and general process information would be great as well.

Thank you
Wraith

RE: Flow drilling??

Wraith,

Are you still looking for information on "thermal drilling"? You can get some good information from:

www.danly-te.com

RE: Flow drilling??

Hi.
I too would like some further information on the flow drilling process. A client has asked me to flow drill holes in 10 mm thick ms columns on site by hand in position. Has anyone come across this site, hand application before?
Many thanks

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources