A444.0 Mechanical properties
A444.0 Mechanical properties
(OP)
Im looking for information on an alloy called A444.0. i would be grateful for mechanical properties and corrosion resistance.
thanks in advance.
thanks in advance.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
A444.0 Mechanical properties
|
A444.0 Mechanical propertiesA444.0 Mechanical properties(OP)
Im looking for information on an alloy called A444.0. i would be grateful for mechanical properties and corrosion resistance.
thanks in advance. Red Flag SubmittedThank you for helping keep Eng-Tips Forums free from inappropriate posts. Reply To This ThreadPosting in the Eng-Tips forums is a member-only feature.Click Here to join Eng-Tips and talk with other members! |
ResourcesWhat is rapid injection molding? For engineers working with tight product design timelines, rapid injection molding can be a critical tool for prototyping and testing functional models. Download Now
The world has changed considerably since the 1980s, when CAD first started displacing drafting tables. Download Now
Prototyping has always been a critical part of product development. Download Now
As the cloud is increasingly adopted for product development, questions remain as to just how cloud software tools compare to on-premise solutions. Download Now
|
RE: A444.0 Mechanical properties
Property F Temper T4 Temper
--------- -------- --------
UTS (MPa) 165 160
YS (MPa) 76 70
elongation (%) 13 21
Hardness (HB) 50
Corrosion 1 1
Corrosion ratings (1-5, 1 is best) based on salt spray performance.
RE: A444.0 Mechanical properties
can you tell me your source for this, as we are trying to source as U.S equivalent of a casting handbook that we use in the UK. THe UK one lists all alloyw, chemical composition, properties, pattern shrinkage, uses etc.
RE: A444.0 Mechanical properties
http://www.asminternational.org
RE: A444.0 Mechanical properties
You should visit the AFS website for reference material of this type. The publications section can be accessed using the following link:
http://www.afsinc.org/estore/Index.asp
RE: A444.0 Mechanical properties