Anyone with some good friction information?
Anyone with some good friction information?
(OP)
I am looking for a table with some co-efficient of friction information. Just close approximations.
Simply dry clean Stainless steel on chrome plated steel (or some other combinations) NO LUBRICATION, chrome is 10-20rms, Stainless is 40-50.
I'd rather not do any testing if I can get away with it.
Also, what is a good surface treatment to reduce Stainless to Stainless galling as higher pressures. We tried Armalloy coating (which is affordable), and the jury is still out.
I need to keep the corrosion resistance of SS, but have minimal $$$ and time to experiment.
Thanks for the help
Simply dry clean Stainless steel on chrome plated steel (or some other combinations) NO LUBRICATION, chrome is 10-20rms, Stainless is 40-50.
I'd rather not do any testing if I can get away with it.
Also, what is a good surface treatment to reduce Stainless to Stainless galling as higher pressures. We tried Armalloy coating (which is affordable), and the jury is still out.
I need to keep the corrosion resistance of SS, but have minimal $$$ and time to experiment.
Thanks for the help





RE: Anyone with some good friction information?
RE: Anyone with some good friction information?
Check out threads:
Thread 367-41402
and
Thread 367-31365
RE: Anyone with some good friction information?
I'm a little slow tonight....how do I go to a specific thread number?
still a new guy to eng-tips
RE: Anyone with some good friction information?
Thread367-31365
No space between "thread" and the number creates a link.
I didn't know that before, now I do!
Cheers
Greg Locock
RE: Anyone with some good friction information?
I did a search and this time I typed in the correct terms and got much better results. Imagine that, the search engine did not read my mind the first try? Seems like friction is a pretty common topic here.
Thanks for the SS info Metalguy