Material for high temperature caustic vessels
Material for high temperature caustic vessels
(OP)
Hi Guys,
I'm designing a pressure vessel with 250 C temperature and 20 barg for caustic soda 50%. Do you have any idea about material selection? I have read a couple of references like "Alloy selection for caustic soda service" and "NACE SP040315" but not applicable for this temperature.
Thanks
I'm designing a pressure vessel with 250 C temperature and 20 barg for caustic soda 50%. Do you have any idea about material selection? I have read a couple of references like "Alloy selection for caustic soda service" and "NACE SP040315" but not applicable for this temperature.
Thanks





RE: Material for high temperature caustic vessels
RE: Material for high temperature caustic vessels
https://e-reports-ext.llnl.gov/pdf/326030.pdf
RE: Material for high temperature caustic vessels
Earlier this posting was posted in "Corrosion Engineering forum". After getting 2 responses including one from myself, suddenly this posting was removed from the above forum and got reposted here.
Any specific reason?
Thanks.
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
ca.linkedin.com/pub/pradip-goswami/5/985/299
RE: Material for high temperature caustic vessels
Steve Jones
Corrosion Management Consultant
http://www.linkedin.com/pub/8/83b/b04
All answers are personal opinions only and are in no way connected with any employer.
RE: Material for high temperature caustic vessels