Hi all I'm new here I've been operating and programming lasers for about 20 years now, but I am stumped. We cut mostly A-36 steel for auto industry equipment so we do not do a lot of fine detail work. I have been asked to make a fairly intricate sign and my parameters are not doing so well. I was wondering if someone could tell me what settings they use for a base to work from. I have a Bystar 3015 6k machine we usually cut with oxygen but also have nitrogen on site. I think the fine detail of this part would cut better with nitrogen but my settings are way off. Thanks in advance.