INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

welder continuity log book

welder continuity log book

welder continuity log book

(OP)

as i understand welder continuity log should be according to welding process.
it means S.A.W process also involved in welder continuity log.
all welding process used by welder in continuity log should mention position of welding.
please correct me if i am wrong.
regards

RE: welder continuity log book

A welder must have used the process within a 6 month period. Position is not relevant as long as he/she/it was qualified for it previously.

RE: welder continuity log book

Agreed with Don56, it is only the process that they must perform within 6 months, it does not matter how they do it.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources