NDT Requirements for SA-182
NDT Requirements for SA-182
(OP)
Dear Experts,
I had to verify MTRs of 1" Sch-160 tee and concentric reducer 3" x 1" Sch-160 material SA-182 F91. NDT mentioned on MTR is Magnetic Testing only. I have following queries:
1. As per SA-182 Clause 13 , NDT is required for DIN 100 and above. Is it true?
2. Are there any hydrotest (or ET as replacement to hydrotest) compulsory requirements for SA-182 fittings?
I had to verify MTRs of 1" Sch-160 tee and concentric reducer 3" x 1" Sch-160 material SA-182 F91. NDT mentioned on MTR is Magnetic Testing only. I have following queries:
1. As per SA-182 Clause 13 , NDT is required for DIN 100 and above. Is it true?
2. Are there any hydrotest (or ET as replacement to hydrotest) compulsory requirements for SA-182 fittings?





RE: NDT Requirements for SA-182
2. No requirement for hydro.
RE: NDT Requirements for SA-182
RE: NDT Requirements for SA-182