INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Material Selection for Gas skid

Material Selection for Gas skid

Material Selection for Gas skid

(OP)

For a turbine gas supply station we have to meet design pressure of 100 barg at a temperature of 60 oC. Could someone advise on material selection for piping. Ase ASME B16.34 material group 1.1 materials sufficient?

RE: Material Selection for Gas skid

ASME B16.34 is for Valves, Flanged, Threaded, and Welding End.

The materials group 1.1 listed in this code is for carbon steel materials which "may" be acceptable in the appropriate pipe code.

however, it is best to investigate the scope diagrams in B31.8 or B31.3 for appropriate use.

my guess would be B31.8.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources