INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Impact test requirement for SS 304L ( -196°C)

Impact test requirement for SS 304L ( -196°C)

Impact test requirement for SS 304L ( -196°C)

(OP)
Dear sir,

I have one of the equipment with -196°C and colder temp. (MDMT)with metallurgy of SS304L.

Pls let me know whether Impact test is required at -196°C, If yes then what will be acceptance criteria for test result.
Furthermore confirm whether Lateral expansion is to be tested.

Regards
Suyog Gawande
Inspection-MECHANICAL

RE: Impact test requirement for SS 304L ( -196°C)

And what is the Code of Construction???

RE: Impact test requirement for SS 304L ( -196°C)

Dear Gsuyog,
Find out the ASTM code for the MOC. You would get your answer there.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources