INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Where is the ACI 318-05 Section 7.10.5.6 in the ACE 318-14?

Where is the ACI 318-05 Section 7.10.5.6 in the ACE 318-14?

Where is the ACI 318-05 Section 7.10.5.6 in the ACE 318-14?

(OP)
I am not finding this for the life of me. Did it go away?

Thanks.

RE: Where is the ACI 318-05 Section 7.10.5.6 in the ACE 318-14?

ACI provides reference documents to convert from ACI 318-11 to 318-14 and vice-versa.

ACI 318-11 section 7.10.5.6 is now in 10.7.6.2.2 in ACI 318-14.

Professional Engineer (ME, NH, MA) Structural Engineer (IL)
American Concrete Industries
https://www.facebook.com/AmericanConcrete/

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources