INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Wide Flange Rolling Tolerances (US)

Wide Flange Rolling Tolerances (US)

Wide Flange Rolling Tolerances (US)

(OP)
I have gone through ASTM A6 a few times and for the life of me I can't locate the tolerance on thickness for flanges and webs of wideflange shapes. Can anyone point me to where they are?

RE: Wide Flange Rolling Tolerances (US)

Because there are so many web and flange thicknesses I don't believe dimensional tolerances are specified. What is specified:

"Area and Weight Variations: + 2.5% theoretical or specified amount"

See the "Standard Mill Practice" section of the Manual of Steel Construction.

www.SlideRuleEra.net idea
www.VacuumTubeEra.net r2d2

RE: Wide Flange Rolling Tolerances (US)

(OP)
Thank you sir. I eventually found the footnote in A6 that confirms it, no specified thickness tolerances, just weight

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources