INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Fracture Mechanics - error in contour integral calculation in abaqus

Fracture Mechanics - error in contour integral calculation in abaqus

Fracture Mechanics - error in contour integral calculation in abaqus

(OP)
Dear Users,
I'm perform some calculations in abaqus/standard with objective of evaluate stress intensity factor K1 through J Integral Method.
I Use triangular quarter point elements (STRIA65) sorrounding the crack tip to represent properly the singularity (1/sqrt(r)) around the crack tip but my simulation shows an error after first increment in *.msg file:
Contribution to contour integral for 16 elements is not included. The elements have been identified in element set ErrElemContribJIntegralStep1Inc1.
The following card has been used in the code:

*Contour Integral, crack name=H-Output-1_Crack-1, contours=5, crack tip nodes, type=K FACTORS
N_crack, N_crack_tip, 1., 0., 0.


Somebody can help me?

Best Regards

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources