Welding 3CR12 Ferritic Stainless Steel
Welding 3CR12 Ferritic Stainless Steel
(OP)
Can anyone tell me what happens to the tensile strength of 3CR12 parent material in the immediate area of a weld.
Does it become normalised. If so, how does this effect the yield stress (normally 320 N/mm^2 min.)
Does it become normalised. If so, how does this effect the yield stress (normally 320 N/mm^2 min.)





RE: Welding 3CR12 Ferritic Stainless Steel
Stainless Steel - NiDI -- The Nickel Development Institute http://www.nidi.org
RE: Welding 3CR12 Ferritic Stainless Steel
The welding of 3CR12 causes embrittlement associated with severe grain growth in the heat affected zone and fusion zone. This will lower mechanical properties such as tensile & yield point.