thread408-205579: Flange Raised Face Height Tolerance
ASME PCC-2-2011
Article 3.5
Flange Repair and Conversion
"Under-thickness of a raised face due to refinishing
shall be acceptable, provided the minimum finished
height of the raised face is 0.8 mm (0.031 in.)".