Table UW-12 of ASME SEC. VIII DIV 1
Table UW-12 of ASME SEC. VIII DIV 1
(OP)
I want to carry out UT in lieu of RT. Table UW-12 indicates joint efficiency values only if joint is radiographed. Where I could get joint efficiency values for UT joints?





RE: Table UW-12 of ASME SEC. VIII DIV 1
RE: Table UW-12 of ASME SEC. VIII DIV 1
Question: Do the joint efficiencies listed in Table UW-12 apply when ultrasonic testing is performed in lieu of radiographic examination, when allowed by UW-51?
Reply: Yes.
Hope this helps.
RE: Table UW-12 of ASME SEC. VIII DIV 1
RE: Table UW-12 of ASME SEC. VIII DIV 1
Jano6924 (Mechanical)- I donot find this interpretation in 2017 edition.
Please help.
RE: Table UW-12 of ASME SEC. VIII DIV 1
RE: Table UW-12 of ASME SEC. VIII DIV 1
RE: Table UW-12 of ASME SEC. VIII DIV 1
Read UW-51(a)(4)
RE: Table UW-12 of ASME SEC. VIII DIV 1
https://cstools.asme.org/Interpretation/SearchInte...
I cannot talk about the 2017 edition of the code I still don’t get it. I understand that an interpretation remains valid until specifically annulled by the code, or implicitly annulled by other interpretation or by a revision or change in a VIII-1 paragraph.
Please take note that per VIII-1-16-89 interpretation the joint efficiencies of Table UW-12 can be used for ultrasonic testing ONLY WHEN ALLOWED BY UW-51.
Regards.
RE: Table UW-12 of ASME SEC. VIII DIV 1