INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Dowels using ACI 318

Dowels using ACI 318

Dowels using ACI 318

(OP)
I am trying to figure out information for rebar in tension (vertical rebars connecting an existing concrete slab to a new concrete section on top). The tensile strength of grade 60 bar is 90 ksi and the yield strength is 60 ksi based on Table 2 of ASTM A615-16.

Currently, I am looking into some work where it is stated that ACI uses 0.75Fu > 0.9Fy, which is 0.75(90 ksi) = 67.5 ksi > 0.9(60 ksi) = 54 ksi. Appreciate your input where in ACI this might be in, I have not been able to locate this information.

Also, based on this information it is being stated that Appendix D in ACI will not be used. Does that seem appropriate?

Thanks


Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources