INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Hardness survey requirement to NACE MR 0175.

Hardness survey requirement to NACE MR 0175.

Hardness survey requirement to NACE MR 0175.

(OP)
Dear Experts,

Please advise on below query.

Applicable codes are;
ASME Section IX
NACE MR 0175.

We have one WPS Qualified in butt joint and Hardness survey done according to NACE MR 0175 (7.3.3.3 Figure 2) on Butt weld coupon.

​Is it correct that we cannot use the above WPS in a fillet joint because the fillet weld harness survey is not carried out.

​Thanks
BAS

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources