Impact test in HAZ for B31.3
Impact test in HAZ for B31.3
(OP)
I am developing PQR for piping.Impact test is required per B31.3.cupon (A333 Gr 6 to A350 LF2)thickness is 32 mm and will be welded by GTAW(8mm)+SMAW(8mm)+SAW(16mm).
Do I need to carry HAZ impact for each process.
If yes, where i will find reference of this in code.For weld I know each impact cupon shall carry weld deposit from each process so top and bottom samples will be required i.e. 2 sets.However I am confused with HAZ impact.
Do I need to carry HAZ impact for each process.
If yes, where i will find reference of this in code.For weld I know each impact cupon shall carry weld deposit from each process so top and bottom samples will be required i.e. 2 sets.However I am confused with HAZ impact.





RE: Impact test in HAZ for B31.3