INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

API 1104 Preheat on WPS

API 1104 Preheat on WPS

API 1104 Preheat on WPS

(OP)
I am trying to write a WPS for 5L 16".844 Grade B using E6010/E8010. I am trying to find information on preheat and maximum interpass temperatures. I don't see anything of reference in 1104. What am I missing here?

RE: API 1104 Preheat on WPS

API 1104 does not specify preheat temperatures, or for that matter, other welding parameters. The Company is required to demonstrate they have the engineering experience and knowledge to develop a welding procedure that is capable of making mechanically sound welds meeting API 1104 Section 5 requirements.


RE: API 1104 Preheat on WPS

(OP)
That was what I needed. Thank you.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources