Fig UCS-66.2
Fig UCS-66.2
(OP)
Folks,
Is tr in Fig UCS-66.2, the UG-27/UG-28 calculation (ta in UG-45) or final tUG-45? If it is UG-27/UG-28, can it be below UG-16 Minimum value?
Thanks.
Is tr in Fig UCS-66.2, the UG-27/UG-28 calculation (ta in UG-45) or final tUG-45? If it is UG-27/UG-28, can it be below UG-16 Minimum value?
Thanks.





RE: Fig UCS-66.2
ta (UG-45) = t (UG-27/28) + CA
Cheers,
gr2vessels
RE: Fig UCS-66.2