INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

hydrometer/salt meter for B117 Recomendations?

hydrometer/salt meter for B117 Recomendations?

hydrometer/salt meter for B117 Recomendations?

(OP)
Hi guys, I'm currently setting up a B117 salt fog test for my company, i am pretty new to this process.
i use a Singleton SCCH Salt fog chamber, and i am looking for a quick and easy way to measure the 4-6% salt content. i saw the glass bulb type of hydrometer (that kinda looks like a fishing bobber)for sodium chloride and thought it was a pretty simple method.

Can anyone recommend a place/brand that worked for them to get one from?
Also if you can recommend a digital salt% meter that would be helpful as well.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources