Column Lap Length and lapping Zone
Column Lap Length and lapping Zone
(OP)
Hello,
At my site, i am facing an issue regarding lap length of column. First, all the laps are just on the slab(at starter point) and second most important, my remaining lap that is left behind for lapping of further column is just 36" and we are using #8 bar.
So, is it ok to provide 36" lap just at the starter zone? if not, then what to do?
please share your opinion.
At my site, i am facing an issue regarding lap length of column. First, all the laps are just on the slab(at starter point) and second most important, my remaining lap that is left behind for lapping of further column is just 36" and we are using #8 bar.
So, is it ok to provide 36" lap just at the starter zone? if not, then what to do?
please share your opinion.






RE: Column Lap Length and lapping Zone
Check out Eng-Tips Forum's Policies here:
FAQ731-376: Eng-Tips.com Forum Policies
RE: Column Lap Length and lapping Zone
RE: Column Lap Length and lapping Zone
I like to debate structural engineering theory -- a lot. If I challenge you on something, know that I'm doing so because I respect your opinion enough to either change it or adopt it.
RE: Column Lap Length and lapping Zone
Is 3feet lap length is enough or not?
RE: Column Lap Length and lapping Zone