SA 516 Gr.70N with HIC
SA 516 Gr.70N with HIC
(OP)
Hi!
I´m searching if it is possible to get plates in SA 516 GR. 70N with HIC?
Thank you
Rolander
I´m searching if it is possible to get plates in SA 516 GR. 70N with HIC?
Thank you
Rolander





RE: SA 516 Gr.70N with HIC
http://www.usa.arcelormittal.com/~/media/Files/A/A...
Regards,
Mike
The problem with sloppy work is that the supply FAR EXCEEDS the demand
RE: SA 516 Gr.70N with HIC
Thus, the answer to your assumed question is: yes, it is possible
Steve Jones
Corrosion Management Consultant
http://www.linkedin.com/pub/8/83b/b04
All answers are personal opinions only and are in no way connected with any employer.
RE: SA 516 Gr.70N with HIC
"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
RE: SA 516 Gr.70N with HIC
http://www.oakleysteel.co.uk/hic-material-for-sour...
Steve Jones
Corrosion Management Consultant
http://www.linkedin.com/pub/8/83b/b04
All answers are personal opinions only and are in no way connected with any employer.