INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

pitting corrosion of duplex stainless steel (A2205) in acetic acid service

pitting corrosion of duplex stainless steel (A2205) in acetic acid service

pitting corrosion of duplex stainless steel (A2205) in acetic acid service

(OP)
We have severe pitting issue in duplex stainless steel (A2205) piping and equipments in CTA plant.
Pitting occurs mostly in the stream containing acetic acid with high bromide content.
Following is the composition of the stream.
Acetic acid: > 70%
Water: 4 – 10%
Catalyst: 1.6 to 3 % (MnBr, Mn-acetate, Cobalt acetate)
Temperature: 90 – 120 degree

Can anyone share his experience, what is maximum permitted bromide content in acetic acid for duplex stainless at above temperature range.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources