Hi,
I've got a RFQ for 4" Pipes, 10m Long with 4" Fig 602 Thd x Wing Weld Ends and the delivery is within 1 Week.
The question is, Whether, Can i Weld the 6m and 4m Pipes together or it should be 10m single Long pipe?
Since i have the 6m Long pipes already in stock.
Service: H2S.
Please advise. Ofcourse, I can ask the customer, but before that i wanted to be sure.
Your reply is really appreciated.
Thanks & Regards
I've got a RFQ for 4" Pipes, 10m Long with 4" Fig 602 Thd x Wing Weld Ends and the delivery is within 1 Week.
The question is, Whether, Can i Weld the 6m and 4m Pipes together or it should be 10m single Long pipe?
Since i have the 6m Long pipes already in stock.
Service: H2S.
Please advise. Ofcourse, I can ask the customer, but before that i wanted to be sure.
Your reply is really appreciated.
Thanks & Regards





RE: 4" Fig 602, 10m Long Pipes
RE: 4" Fig 602, 10m Long Pipes
RE: 4" Fig 602, 10m Long Pipes
will the client accept it? No idea.
Can you weld and supply in the time frame?
Offer it and see.
Or provide both options. If 4m and 6m pipes joined are faster delivery and cheaper then.....
Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
RE: 4" Fig 602, 10m Long Pipes
Thank you for your response.
@LittleInch
I'll do it like you said.
Thanks.
Thanks & Regards