INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AC1 and AC3 in AISI410 Material

AC1 and AC3 in AISI410 Material

AC1 and AC3 in AISI410 Material

(OP)
Hi All,

I am trying to find out the values for the AC1 and AC3 for AISI410 material

A formula was submitted on here many years ago, but it was stated not to work for steels with high Cr contents.

If someone can point me in the general direction of a reasonably accurate formula or typical figures for this grade, it would be much appreciated

Thanks

RE: AC1 and AC3 in AISI410 Material

(OP)
Thanks for that metengrthumbsup2

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources