Nickel alloys list
Nickel alloys list
(OP)
Hi,
Does anyone knows how can I find some complete list of all nickel and Ni/Fe alloys? A list of all Ni UNS numbers alloys maybe could help me too.
Thanks.
Jean Silva.
Does anyone knows how can I find some complete list of all nickel and Ni/Fe alloys? A list of all Ni UNS numbers alloys maybe could help me too.
Thanks.
Jean Silva.





RE: Nickel alloys list
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
RE: Nickel alloys list
RE: Nickel alloys list
Another reference...
METALLIC MATERIALS SPECIFICATION HANDBOOK, Robert Ross, Chapman & Hall [I have 4th Ed, ISBN, 0-412-36940-0].
All UNS alloy numbers and their common-alloy numbers/designations and their procurement specs are listed in Chapter 27 Nickel [Ni] alloys. This book includes EXACTLY what you are ASKING for.
CAUTION. Actual physical/mechanical/etc properties are NOT listed in this document... more research required.
Regards, Wil Taylor
o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
RE: Nickel alloys list
ATI
SMC
VDM
The full UNS list is every alloy that has an assigned number, many of them are not available.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
RE: Nickel alloys list