INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

why pipe material(SA 106 Gr.B) do not contain any sign Like SA 516 Gr70N & SA 105N

why pipe material(SA 106 Gr.B) do not contain any sign Like SA 516 Gr70N & SA 105N

why pipe material(SA 106 Gr.B) do not contain any sign Like SA 516 Gr70N & SA 105N

(OP)
Good to see you again,

I have a one doubt why the pipe material do not contain normalized sign(SA 106 Gr.B N)

please reply me

RE: why pipe material(SA 106 Gr.B) do not contain any sign Like SA 516 Gr70N & SA 105N

ramesh349, this pipe is generally not normalized. Refer the specification, SA-106.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand

RE: why pipe material(SA 106 Gr.B) do not contain any sign Like SA 516 Gr70N & SA 105N

It can actually be quite difficult sometimes to find SA-106 in normalized condition. If you want a normalized pipe, you're sometimes better off just specifying another grade such as SA-333-6.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources