INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

I am back looking for an aluminium

I am back looking for an aluminium

I am back looking for an aluminium

(OP)
I am back looking for an aluminium specification for EN44100, I have tried MATWEB but, got no joy, any help would be appreciated.

regards

RE: I am back looking for an aluminium

Some welding data charts mention this alloy.  I believe it is european, and reference is made to similarity of 4043 alloy.  Not much to go on, but I hope this helps.

RE: I am back looking for an aluminium

EN 1706 exists as either BS EN 1706 or DIN EN 1706:
Aluminium and aluminium alloys - Castings
Chemical composition and mechanical properties


The full designation is either EN AC-44100 or EN AC-Al Si12(b).  It has the following composition:

Si = 10.5-13.5
Fe = 0.65 (0.55 for ingot)
Cu = 0.15 (0.10 for ingot)
Mn = 0.55
Mg = 0.10
Ni = 0.10
Zn = 0.15
Pb = 0.10
Ti = 0.20 (0.10 ingot)
Al = remainder

You can obtain a copy of this standard from Global Engineering Documents or BSI using the following links:

http://global.ihs.com

http://bsonline.techindex.co.uk/

RE: I am back looking for an aluminium

(OP)
Once again TVP you come up trumps.

Thanks alot.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources