Defference between ASTM A105 and ASTM A234
Defference between ASTM A105 and ASTM A234
(OP)
Hi Guys,
I just want to know what is the differences between ASTM A105 and ASTM A234.
I have choose ASTM A234 for my utility water line, but supplier supply to me ASTM A105, so is that ok?
thank you.
Best Regards,
Antonio.
I just want to know what is the differences between ASTM A105 and ASTM A234.
I have choose ASTM A234 for my utility water line, but supplier supply to me ASTM A105, so is that ok?
thank you.
Best Regards,
Antonio.





RE: Defference between ASTM A105 and ASTM A234
What size range are you using?