Welding consumables for A694 F65
Welding consumables for A694 F65
(OP)
Can anybody suggest welding consumables for GTAW, SMAW & SAW process for welding of A694 F65 to itself and A694 F70 to itself.thickness is 32 mm and PWHT is required per B31.3 code.
Service is SOUR so Ni% in weld consumables is required below 1%.
Please suggest??
Service is SOUR so Ni% in weld consumables is required below 1%.
Please suggest??





RE: Welding consumables for A694 F65
RE: Welding consumables for A694 F65