dual certified material, A312 316/316L
dual certified material, A312 316/316L
(OP)
In a dual certified material, A312 316/316L : where
316 has good mechanical mechanical strength (because of Nickel)
316 L (Low carbon) (Less hardness)
Is that the reason for choosing 316L/316?
316 has good mechanical mechanical strength (because of Nickel)
316 L (Low carbon) (Less hardness)
Is that the reason for choosing 316L/316?





RE: dual certified material, A312 316/316L
RE: dual certified material, A312 316/316L
http://www.eng-tips.com/search.cfm?q=dual+certifie...
Steve Jones
Corrosion Management Consultant
http://www.linkedin.com/pub/8/83b/b04
All answers are personal opinions only and are in no way connected with any employer.
RE: dual certified material, A312 316/316L