T12-150 rebar mean ???
T12-150 rebar mean ???
(OP)
what does T12-150 re bar mean ???
T12 mean 12 mm diameter re-bar and 150 is c/c spacing ?
T12 mean 12 mm diameter re-bar and 150 is c/c spacing ?
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: T12-150 rebar mean ???
T12-150 means 12mm diameter high yield bar (Grade 460 to BS4449) at 150mm centres. You don't show a bar mark so I assume the 150 is the spacing.