INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASTM A358 Class 3 vs. Class 1

ASTM A358 Class 3 vs. Class 1

ASTM A358 Class 3 vs. Class 1

(OP)
Hello,

I asked during bid phase an ASTM A358 Class 1 pipe. The Vendor offered the Class 3 instead.

The only difference is that Class 1 is a double welded pipe whereas Class 3 is single welded pipe. Both pipes are 100% radiographed.

Any of you see any concern to accept this deviation, namely Class 3 instead of Class 1? I don't see any.

Thank you and regards.

EStilli, Piping Material Engineer

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources