INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

What water type is best for topping up ni-cad cells?

What water type is best for topping up ni-cad cells?

What water type is best for topping up ni-cad cells?

(OP)
Hi,

Was wondering what types of water is best for topping up UPS nickel-cadmium cells?

We have steam condensate water and treated water available, treated water has been through reverse osmosis.

Any suggestions would be much appreciated.

RE: What water type is best for topping up ni-cad cells?

How pure is your condensate? Most boilers are dosed with oxygen scavenger, inhibitors, and so on. RO water should be OK, but again check your purity.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources