Molded-fiber/pulp Packaging Design Tips
Molded-fiber/pulp Packaging Design Tips
(OP)
Been using Google the past hour, but have not found any design recommendations for molded-fiber or molded-pulp packaging inserts. Seems like this information is being held tight to the chest of the suppliers. Does anyone have links to good design resources? Looking for material thickness to product weight ratios, required draft angles, tonnage requirements based on area of insert, etc.
"Art without engineering is dreaming; Engineering without art is calculating."
Have you read FAQ731-376: Eng-Tips.com Forum Policies: Eng-Tips.com Forum Policies to make the best use of these Forums?





RE: Molded-fiber/pulp Packaging Design Tips
http://www.iopp.org/files/public/HoweEmilyRIT.pdf
"Art without engineering is dreaming; Engineering without art is calculating."
Have you read FAQ731-376: Eng-Tips.com Forum Policies: Eng-Tips.com Forum Policies to make the best use of these Forums?