AWS D1.4 PQR Position Essential Variable
AWS D1.4 PQR Position Essential Variable
(OP)
In the 1998 and 2005 D1.4, the table for essential variables includes a change in position not qualified per 6.2.4 which implies any change in position requires a new PQR. However, the 2011 edition's table of essential variables references 6.3.4 which is in the section for welder qualifications. I am wondering if the 2011 is in error or if using the welder qualification requirements is appropriate. Or, am I missing something else?
This came up when contractor asked if they could use 3G and 4G PQRs to qualify a WPS for a horizontal flare bevel groove weld joint (indirect butt joint with a splice plate). For welder qualifications and the 2011 edition, the 3G PQR looks like it will work.
This came up when contractor asked if they could use 3G and 4G PQRs to qualify a WPS for a horizontal flare bevel groove weld joint (indirect butt joint with a splice plate). For welder qualifications and the 2011 edition, the 3G PQR looks like it will work.