Iso 15608 group number to Asme ix
Iso 15608 group number to Asme ix
(OP)
We currently used en10025 s275jr ISO 15608 group number 1.1 on our storage tanks. But at the moment we dont have any specific WPS for this unassigned material. We do have a wps for SA283 GR C which have the same ISO 15608 group number as EN10025 S275JR which is 1.1. Can i just use this ISO group number as a justification so that i can use SA 283 wps for this purpose.





RE: Iso 15608 group number to Asme ix
EN10025 S275JR has not been assigned a P number so therefore it is classed as "Un-assigned" and requires a new WPS / PQR,
Regards,
DD
RE: Iso 15608 group number to Asme ix