Hi,
we are trying to take the replica of U duct made up of INCONEL material. What is the most appropriate etchant for INCONEL Alloys?
What are the possible phases and microsturcture and which damage mechanisms may occur to this alloy?
Please help.
we are trying to take the replica of U duct made up of INCONEL material. What is the most appropriate etchant for INCONEL Alloys?
What are the possible phases and microsturcture and which damage mechanisms may occur to this alloy?
Please help.





RE: Replica of INCONEL alloy
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
RE: Replica of INCONEL alloy
RE: Replica of INCONEL alloy
First, you can search on your own and find plenty of information on microstructure and associated damage mechanisms. See below to name a few
http://www.aerospacelab-journal.org/sites/www.aero...
Another
http://www.tms.org/superalloys/10.7449/1994/Supera...
http://www.dtic.mil/dtic/tr/fulltext/u2/466476.pdf
Second, regarding etching behavior, see the link below
http://vacaero.com/information-resources/metallogr...