INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Recommendation of Bolting Material for 600# Stainless Steel Piping Class applied NACE MR0103

Recommendation of Bolting Material for 600# Stainless Steel Piping Class applied NACE MR0103

Recommendation of Bolting Material for 600# Stainless Steel Piping Class applied NACE MR0103

(OP)
Dear Sirs,

Please give recommendation of bolting material considering followings.

1. Low strength bolting materials are limited to class 150 and class 300 in accordance with note 4 of table 1B in ASME B16.5.
Quote " These bolting materials may be used with all listed materials but are limited to Class 150 and Class 300 joints. See para. 5.3.4 for recommended gasket practices." unquote

2. ASTM A193 Grade B8MA, Class 1A is specified in Table 9 of NACE MR0103-2013 edition as material meeting the requirement of section 2.

SSC is mainly related to material strength and high hardness is main reason for susceptibility to SSC.

So, please give recommendation bolting material which meets the requirement of NACE MR0103 and is applied to 600# Class.

Thanks for your reply in advance.



RE: Recommendation of Bolting Material for 600# Stainless Steel Piping Class applied NACE MR0103

a) Is the bolting exposed, or unexposed?

b) Are you comfortable with unexposed bolting of low alloy steel in a stainless steel piping system?

Steve Jones
Corrosion Management Consultant

http://www.linkedin.com/pub/8/83b/b04

All answers are personal opinions only and are in no way connected with any employer.

RE: Recommendation of Bolting Material for 600# Stainless Steel Piping Class applied NACE MR0103

(OP)
Dear Steve Jones

Thanks for your reply.

a) Is the bolting exposed, or unexposed?

Exposed

b) Are you comfortable with unexposed bolting of low alloy steel in a stainless steel piping system?

And Owner wants to apply stainless bolting material to Stainless steel piping applied NACE MR0103.


If you have further inforamtions, please feel free to let me know.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources