INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

NICR-A weld on N06625(GTAW)

NICR-A weld on N06625(GTAW)

NICR-A weld on N06625(GTAW)

(OP)
Hi Team,

Recently we weld with Nicr-A on N06625 using GTAW but at the end of welding, we found cracks.
So, we grind the crack area & re-weld. But, Crack become worse.

Need before & after weld guide and advise to avoid crack.

Thanks.

RE: NICR-A weld on N06625(GTAW)

Can you tell us what is Nicr-A filler metal? Also, what type of weld?

RE: NICR-A weld on N06625(GTAW)

Exact composition needed, as there are about 200 alloys with names that start with "NICR".

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources