Moment of inertia for PVC Pipe
|
RE: Moment of inertia for PVC Pipe
see: http://www.matweb.com/search/SpecificMaterial.asp?bassnum=O5601
Tensile Modulus 1.124 - 4.827 GPa 163 - 700 ksi Average = 2.7 GPa; Grade Count = 27
Flexural Modulus 1.296 - 4.689 GPa 188 - 680 ksi Average = 2.8 GPa; Grade Count = 25